Factors that can cause hydrogen cracks

A hydrogen crack is a delayed crack that normally forms after welding when the temperature in the joint drops below +200 °C (392 °F). A crack can initiate and develop hours after welding is finalized. Detection of potential cracks is normally made 16—48 hours after the completion of welding. The actual time depends on standard requirements or a separate agreement.

There are three key factors influencing the risk of hydrogen cracks:

  • The presence of a brittle microstructure in the joint (alloy elements)
  • Hydrogen content in the joint
  • Tensile stresses in the joint

The forming of a brittle microstructure in the weld is strongly dependent on the alloy content in the base and filler materials and on the cooling rate. The hydrogen is introduced mainly from moisture and dirt but also by the filler material and is very dependent on the type of filler used. Tensile stresses always occur in welded joints to some extent because of the thermal shrinkage during cooling and the degree of constraint in the design of the joint. These key factors all interact with each other. For example, if the hydrogen content is increased in the joint for a specific welding situation, the cracks can form at lower tensile stresses. Different models exist on how these three parameters interact with each other. However, no exact proven mechanism for the initiation of hydrogen cracks exists.

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026