4 min read

Product
Hardox® 500 TufCountry
Austria
Company
Industry
Brand program
Hardox® In My Body
Winkelbauer GmbH in Austria is a leading supplier of heavy-duty buckets and other construction equipment for the European market. The company is an early adopter of SSAB’s new wear-resistant steel grade Hardox® 500 Tuf. Upgrading to this material allows Winkelbauer’s customers to load more and extend the service life of their equipment.
By using Hardox® 500 Tuf in a thinner dimension, the new generation of Winkelbauer heavy-duty buckets has 10-16% less tare weight with the same service life as the previous generation. This allows for an increase of loaded volume by 6-10% at the same total weight.
To meet a particular customer’s request, Winkelbauer designed a bucket that allows the operator to load a truck to its maximum capacity of 24 tons (52,911 lbs.) with only 3 turns. This saves 25% of the time required for a loading cycle, and the operator knows that 3 full buckets are enough.
I’m interested in Hardox® 500 Tuf. Contact me
Hardox® 500 Tuf in thinner dimensions gives the new generation of Winkelbauer heavy-duty buckets up to 16% less tare weight with the same service life as the previous generation.
Hardox® 500 Tuf combines the best properties from the Hardox® 450 and Hardox® 500 wear steel grades. It has a guaranteed impact energy of 27 J at -20°C (20 ft-lb at 4°F) and, for 20 mm plate, a typical value of 45 J at -40°C (20ft-lb at 4°F). It also has an unusually narrow hardness window of 475-505 HBW. The estimated relative service life for Hardox 500 Tuf is 85-100% longer than for Hardox® 400 according to SSAB’s wear calculation software WearCalc, based on sliding wear with granite.
Order trial materialWinkelbauer is impressed not just by the quality of the new steel grade, but by SSAB’s unwavering commitment to support and service life.
“We would generally need a timeframe of 1-2 years for a conventional test of a new material. We don’t have that time, which is why we need a partner we can trust and rely upon. The depth of service that we have enjoyed from SSAB employees from the very outset is one-of-a-kind, and this level of quality cannot be found in any competing products on the market. When SSAB releases a material, we know for sure it delivers as promised,” says Michael Winkelbauer.
The welding and machining of Hardox® 500 Tuf can be performed with the same kind of equipment used for other Hardox® grades. Bendability recommendations are similar to those for Hardox® 450.
“Before going into production, we have naturally experimented with the material and tested it in welding. Since it’s important to reduce welding seams in order to minimize production costs and improve performance, we have analyzed wear patterns and modified the design and construction of our buckets to make best possible use of the mechanical properties offered by Hardox 500 Tuf,” says Michael Winkelbauer.
I’d like my own design consultation with SSAB’s experts
With the new design of a heavy-duty bucket in Hardox® 500 Tuf, 24 tons (52,911 lbs) of bulk goods can be loaded in just 3 loads without exceeding the total bucket weight specified by the manufacturer.
Hardox® 500 Tuf is perfectly suited for making hard-working buckets of all sizes and shapes. The bucket will last longer and keep its original shape thanks to the wear steel’s combination of high strength, extreme hardness and guaranteed toughness.



”Hardox® wear plate is absolutely the best material for our buckets”, says Jukka Karhula, CEO of Häggblom Oy.
Read the article

Lower fuel consumption, high durability, increased efficiency and overall longer bucket lifetime with less hassle due to repairs and downtime.
Read Sjørring’s full story