4 min read

Recycling creates some of the toughest operating environments for equipment and machinery components. Glass recycling, one of the most common recycling practices, comes with many challenges. Hardox® Extreme in glass recycling equipment delivers extreme performance so you can keep your glass recycling equipment up and running longer.
Doing away with waste isn’t just about handling the waste that equipment eats up every day – it’s also about wasted time and money due to equipment downtime. Many recycling and recovery professionals are finding that one source of waste they can control is the quality of the equipment they operate.
To remain competitive, glass recyclers have got to minimize equipment wear. As a result, they are constantly looking for an optimal balance between service life and lifecycle cost.
The wear-resistant materials used in glass recycling equipment and plants – such as ceramics and chromium carbide overlay plates – have high wear resistance. But they are expensive, both to purchase and to maintain. So simply achieving the longest service life is not an appropriate strategy to ensure profitability. Lifecycle cost also has to be taken into account. This is given by the cost of the equipment and its maintenance divided by its service life. A third factor is maintenance – the cost of materials and labor to keep the equipment operational.
Also, no dust from the wear-resistant material must be allowed to degrade the finished product.

SSAB’s commitment to making extremely clean steels enables us to offer a product that far outperforms typical 450-500 HBW wear-resistant steels. With a nominal hardness of 60 HRC (Rockwell) and a typical hardness of 650-700 HBW, SSAB’s Hardox® Extreme – the world’s hardest wear plate – meets the demanding requirements of glass recycling plants.
To fully understand the abrasive environment of glass recycling and the performance of different wear-resistant materials, SSAB developed its own wear test for crushed glass. Some of our findings were even published in the special issue of the journal Wear for the 20th International Conference on Wear of Materials in Toronto.
The SSAB wear test rig consists of an 800 x 100 mm (3.15 x 3.94”) steel drum with up to 34 samples placed in a holder mounted around the internal circumference of the drum. All tests were conducted under the same conditions.
A number of wear-resistant materials were tested under sliding wear conditions using crushed glass from a glass recycling plant in Sweden. The test revealed that SSAB’s wear-resistant grade Hardox® Extreme performed well, outperforming materials such as chromium carbide overlay.





Let us show you how this SSAB Ecoupgraded waste-transfer trailer saves fuel and CO2 during its lifetime, and also during the steel production. “SSAB Ecoupgraded” means that equipment has been upgraded with high-strength steel for higher performance and less environmental impact.
Detailed fuel and CO2 savings

Hardox® Extreme is the world’s hardest wear plate with a nominal hardness of 60 HRC (Rockwell) and typical hardness of 650-700 HBW.
Hardox® Extreme product informationThe Australian company Pacific Shredder designs and builds steel shredding machines that can shred a car into scrap in seconds.
Read the article
Recycling creates some of the toughest operating environments for equipment and machinery components. On any given day, machines might grapple with extreme loads, dust contamination, falling debris and temperature fluctuations. And lots of these workhorses are in sore need of that tender loving care called proper maintenance.
Read the article