SSAB Domex 355ML is a thermomechanically rolled structural steel plate that provides high strength at low temperatures. SSAB Domex 355ML meets or exceeds the requirements of S355ML in EN 10025-4.
SSAB Domex 355ML is available in thicknesses of 6.00-63.00 mm and in widths up to 3300 mm depending on the thickness. More detailed dimensions are provided in the dimension program.
The tensile test is made transverse to the rolling direction in compliance with EN 10025-4.
The impact test is made longitudinally to the rolling direction in compliance with EN 10025-4.
SSAB Domex ML products are delivered with tolerances that correspond to ¾ of EN 10029 Class A as default value.
Width tolerances -0/+4-10 mm depending on the thickness. Length tolerances -0/+15-75 mm depending on length.
Tolerances according to EN 10029.
Maximum flatness deviation 6 mm/m as plate.
According to EN 10163-2 Class A, Subclass 3.
Thermomechanically rolled (M).
Minimum inner bending radius is 1.0 x t transverse to the rolling direction and 1.5 x t longitudinal to the rolling direction up to max 20mm in thickness.
For information concerning fabrication, see SSAB´s brochures on www.ssab.com or consult Tech Support.
Appropriate health and safety precautions must be taken when bending, welding, cutting, grinding or otherwise working on the products.