Steel Processing

At the Steel Service Center in Ghedi, steel processing is carried out by highly skilled personnel, with rigorous checks at every stage of the process.

Our Cut to Length line can transform HR steel grades with a yield strength of up to 700 MPa, accommodating thicknesses up to 16 mm and widths up to 2000 mm.

Additionally, through an integrated system of subcontractors, we also provide services such as pickling, slitting, shear blanking, and processing of cold-rolled and metal-coated cut to length.

Cut to length line

  • 13.000 m2 covered area, out of a total of 25.000 m2
  • At least 20 cold, hot, black and pickled high-strength steel grades
  • 200 combinations grades/thicknesses/width in stock up to 1300 MPa yield strength 
  • 80 m the length of the Cut to Length line

Cutting capability

  • up to 12 m in length and up to 2 m in width 
  • from 3.00 to 16.00 mm thickness 
  • HR steel grades up to 700 MPa yield strength
Cut-to-length line
Steel plates.

The right materials for the job

We are experts in the processing of high-strength and special steels, like SSAB Boron®, Strenx® performance steel, Hardox® wear plate, SSAB Domex®, Docol® and SSAB Laser®