Product Name

Armox® 370T Class 1

Dimensions
T: 3.0 - 100.0 mmT: 0.118 - 3.937 in
Hardness
300 - 430 HBW
Standards
EN 10029
Datasheet
Product Name

Armox® 370T Class 2

Dimensions
T: 3.0 - 152.0 mmT: 0.118 - 5.984 in
Hardness
280 - 330 HBW
Standards
EN 10029
Datasheet
Product Name

Armox® 440T

Dimensions
T: 4.0 - 80.0 mmT: 0.157 - 3.150 in
Hardness
420 - 480 HBW
Standards
EN 10029
Datasheet
Product Name

Armox® 500T

Dimensions
T: 3.0 - 130.0 mmT: 0.118 - 5.118 in
Hardness
470 - 540 HBW
Standards
EN 10029
Datasheet
Product Name

Armox® 520T

Dimensions
T: 4.0 - 50.0 mmT: 0.157 - 1.969 in
Hardness
500 - 550 HBW
Standards
EN 10029
Datasheet
Product Name

Armox® 560T

Dimensions
T: 5.0 - 15.0 mmT: 0.197 - 0.591 in
Hardness
530 - 590 HBW
Standards
EN 10029
Datasheet
Product Name

Armox® 600T

Dimensions
T: 4.0 - 20.0 mmT: 0.157 - 0.787 in
Hardness
570 - 640 HBW
Standards
EN 10029
Datasheet
Product Name

Armox® 620T

Dimensions
T: 5.0 - 15.0 mmT: 0.197 - 0.591 in
Hardness
55 - 60 HRC
Standards
EN 10029
Datasheet
Product Name

Armox® Advance

Dimensions
T: 4.0 - 7.9 mmT: 0.157 - 0.311 in
Hardness
58 - 63 HRC
Standards
EN 10029
Datasheet
Product Name

Armox® 500 AM Powder

Dimensions
-
Hardness
500 HBW
Standards
-
Datasheet

Ramor

Product Name

Ramor® 450

Dimensions
T: 8.00 - 16.00 mmT: 0.315 - 0.630 in
Hardness
400 - 480 HBW
Standards
EN 10029
Datasheet
Product Name

Ramor® 500

Dimensions
T: 2.0 - 30.0 mmT: 0.079 - 1.181 in
Hardness
490 - 560 HBW
Standards
EN 10029, EN 10051
Datasheet
Product Name

Ramor® 550

Dimensions
T: 3.0 - 15.0 mmT: 0.118 - 0.590 in
Hardness
540 - 600 HBW
Standards
EN 10029, EN 10051
Datasheet
Product Name

Ramor® 600

Dimensions
T: 3.0 - 6.0 mmT: 0.118 - 0.236 in
Hardness
570 - 640 HBW
Standards
EN 10051
Datasheet
Product Name

Ramor® SR500

Dimensions
T: 4.8 - 12.7 mmT: 0.188 - 0.500 in
Hardness
500 - 590 HBN
Standards
ASTM A6
Datasheet
Product Name

Preliminary Ramor® 500W

Dimensions
T: 4.0 - 6.5 mmT: 0.16 - 0.26 in
Hardness
490 - 560 HBW
Standards
EN 10051
Datasheet