Product Name | Dimensions | Standards | Datasheet |
|---|---|---|---|
| SSAB Weathering Tube 355WH | Circular: 48.3 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.90 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in | EN 10219-2, EN 1090-2 | |
| SSAB Weathering Tube 500WH | Circular: 48.3 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.90 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in | EN 10219-2 | |
| SSAB COR-TEN B Tube | Circular: 48.3 - 323.9 mm Square: 40x40 - 300x300 mm Rectangular: 50x30 - 400x200 mm Wall Thickness: 2.0 - 12.5 mmCircular: 1.90 - 12.75 in Square: in Rectangular: in Wall Thickness: 0.079 - 0.492 in | EN 10025-5, EN 10219-2 |
SSAB Weathering Tube 355WH
SSAB Weathering Tube 500WH
SSAB COR-TEN B Tube
Product name | Dimensions | Standards | Datasheet |
|---|---|---|---|
Several shape possibilities and customer-specific lengths. More information from SSAB Sales. | EN 10162 |