How to weld > Shielding gas

Carbon dioxide (CO₂)

The CO₂ also contributes to a higher capacity of heat transfer to the liquefied melt, which influences the geometry of the weld metal.

 It helps to give the weld metal a relatively large and round shape which is illustrated in the illustration below. The shape and size of the weld metal provides further resistance to lack of fusion and porosity in the weld metal.

Penetration performance of a shielding gas consisting of only CO2.

CO2 is normally added in relatively small amounts. If the CO2 content in the shielding gas is too high, it will obstruct the formation of spray arc welding. The maximum CO2 content under which spray arc welding is feasible in Ar/CO2 mixtures is approximately £ 25%.

The carbon dioxide in the Ar/CO2 shielding gas mixtures stabilizes the arc.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 

Copyright 2026