How to weld > Shielding gas

Selection of shielding gas for MAG welding

Due to the influence of the shielding gas, the final welding performance is a combination of the properties from each individual gas component.

An increased fraction of a gas component leads to a greater influence of the characteristics for that specific gas.

The typical penetration profiles for different gas mixtures are illustrated below in the illustration below for the welding of fillet joints.

Schematic penetration profiles when varying the composition of the shielding gas during MAG welding: a) Ar+ and 2% CO2. b) Ar+ and 5% CO2. c) Ar+ and 10% CO2. d) Ar+ and 20% CO2. e) 100% CO2.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 