How to weld > Shielding gas

Shielding gas for TIG welding

The shielding gas mixture for TIG welding is easier to decide since there are fewer options compared to MAG welding.

During TIG welding, a gas should be used to:

  • Protect the weld pool from the oxygen and nitrogen in the surrounding air
  • The immediate adjacent parent metal to the weld pool
  • Protect the tungsten electrode from oxidation
  • Allow for a stable arc to be established

In general, SSAB proposes a shielding gas composition of pure argon for TIG welding which fulfills these requirements.

Category and tags

How to weldShielding gas

Contact Technical support


The information in this report is only applicable to SSAB’s products and should not be applied to any other products than original SSAB products. 


This report provides general results and recommendations for SSAB steel products. This report is subject to SSAB’s Terms of Use. It shall be the user's responsibility to verify that the information contained herein is correct and is suitable to be used for the particular purpose and application of the user. The report is intended to be used by professional users only who possess adequate expertise, qualification and knowledge for the safe and correct use of the results and recommendations in this report. This report is provided “as is”. The use of the report is at user’s own discretion and risk and that users will be solely responsible for any use of this report. SSAB disclaims any liability for the content or potential errors of this report, including but not limited to warranties and condition of merchantability or fitness for a particular purpose or suitability for individual applications. SSAB shall not be liable for any kind of direct or indirect damages and/or costs related to or arising therefrom, whether special, incidental, consequential or directly or indirectly related to the use of, or the inability to use, the report or the content, information or results included therein. 