When the SSAB steel mill in Oxelösund, Sweden, was looking for a new heat-resistant material in its coke plant, it didn’t have to look far. The solution was right in front of it: Hardox® HiTemp. SSAB developed this particular grade of Hardox® wear plate for abrasive conditions in high heat environments. And it doesn’t get much hotter than in a steel mill’s coke plant.

1.000 tonnes (1,102 tons) of coke per day is the average production at the mill. When the 1.000°C (1,832°F) coke comes out of the coal furnaces, it’s cooled with water and dumped on the sliding ramp – still at a very high temperature.
SSAB has so far been using 40 mm (1.575”) thick basalt ceramic tiles, 300 x 300 mm (12 x 12”), on the sliding ramp, which measures 34 by 5 m (112’ by 16’). The tiles have a lot of drawbacks, apart from being highly expensive. They are prone to cracking, resulting in maintenance stops as often as every three months with 2-3 days of downtime.
Having maintenance personnel working in the coke plant for several days is a health and safety issue. The properties of Hardox® HiTemp promised to change this. SSAB came up with the solution to replace the ceramic tiles on the sliding ramp with steel plates that are 1,940 by 5,000 mm (76.4 by 196.9”) and 20 mm (0.787”) thick. This solution not only improves working conditions, it also allows the production to run uninterrupted.
Installing the plates of Hardox® HiTemp high-temperature steel along the 34 m (112’) ramp was done during a scheduled maintenance stop. Based on experience from other steel tests, SSAB estimates that the ramp fitted with Hardox® HiTemp will operate for up to 14 years without requiring any significant maintenance. This means the maintenance crew will no longer have to change tiles in this hazardous environment, allowing production to run uninterrupted for many years.


In coke plants, Hardox® HiTemp is a cost-effective and long-lasting solution and not just for the sliding ramp as in this case – it can also be used on quenching wagons, cooling beds, slag tippers, furnace inlet scrapers and other heat-affected equipment.
Here are other applications for Hardox® HiTemp high-temperature steel:
Hardox® HiTemp is a quenched and tempered martensitic wear plate with a typical hardness of 375 HBW. Its high toughness, bendability and weldability make Hardox® HiTemp an outstanding choice for a wide range of heat-exposed applications. It can withstand temperatures up to 500°C (930°F) for an extended time without losing its properties. Hardox® HiTemp can be thermally cut without pre-heating thanks to its low carbon equivalent, which also makes it suitable when a lot of welding is required.
I want to know more about Hardox® wear plate – contact me
Hardox® HiTemp is a high-heat grade of Hardox® wear plate that provides a cost-efficient solution for wear resistance at high temperatures in the 300-500°C (570-930°F) range.
Get Hardox® HiTemp product information.jpg%3Fm%3D20221021084122&w=3840&q=75)
Can your dump trucks take the heat? The abrasive wear? When Altus switched from mild steel to Hardox® HiTemp in its slag trucks, it virtually eliminated repairs, and got truck bodies that weigh 40% less.
Read the full story
Subscribe today and receive the latest information about Hardox® wear plate.
Sign up for newsletter