Steel Pile News

Updated Design and installation manual for RD® pile wall

June 18, 2026 10:31 CEST
Welding inspection requirements for the attachment welds of connectors have been updated.

Table 12 of the manual presents the welding requirements according to the execution standard EN 12063 for retaining walls. The table has been updated regarding the attachment welds of the connectors. The new table differentiates between fillet welds and lap joints.

Connectors which can be attached by means of fillet welds include, for example, RM, RF, E21 and LBP180-10 profiles. The lap joint is used with the E22 connector, which has a section at its base parallel to the surface of the pile pipe.

Different fastenings have different inspection requirements according to EN 12063, which are now clearly separated into their own rows in Table 12.

The updated Table 12 of the manual

Where to download

All the downloadable material related to SSAB pile products can be downloaded from the below pages:

In English  

In Finnish 

In Swedish    

More information on RR® and RD® piles and RD® pile wall can be found from www.ssab.com/infra

 

Attachments

Related articles

Other newsESL Shipping and SSAB’s port operations in Raahe develop safety together
Safety, Raahe
Other press releasesSSAB and partners launch closed loop steel recycling initiative in the U.S.
Sustainability, SSAB Americas, Fossil-free steel, SSAB Zero
Steel Pile NewsA completely new function in PileCalc